Kowane takardar zance yana da ginshiƙai biyu, kuma ginshiƙin zinc-nickel koyaushe yana da ƙari. Ga gajeriyar amsa ta farko: biya kuɗin zinc-nickel plating lokacin da kayan aikin ku suka ga yanayi, gishiri ko wankewa. Kasance tare da madaidaicin platin zinc lokacin da suke zaune a gida akan ƙayyadadden rukunin wutar lantarki. Shawarar zinc-nickel vs zinc plating shawarar ba game da matakan inganci ba ne. Yana da kusan layi biyu daban-daban na plating, kuma kuɗin da kuke kashewa yana ƙasa a wurare daban-daban akan kowannensu.
Injiniyan kulawa da ke maye gurɓatattun adaftan a cikin shekara ta biyu ya riga ya biya farashin hasashe ba daidai ba. Wannan labarin yana nuna ainihin abin da ke faruwa a cikin kowane layi a Ruihua Hardware, abin da lambobin gishiri ke nufi, da kuma inda haɓakawa ke samun ci gaba.
Daidaitaccen platin zinc tare da wuce gona da iri shine zaɓin da ya dace don yawancin aikin hydraulic na cikin gida. Shagunan injuna, tsire-tsire masu yin allura da layin sarrafa abinci suna gudanar da yanayi mai tsabta. Kayan aiki akan kafaffen fakitin wutar lantarki ba kasafai suke ganin hazo gishiri ba. Ga waɗancan da'irar, ƙarin kuɗin yana cikin aikin tacewa da juzu'i, ba cikin sutura ba.
Zinc-nickel yana samun ƙimar sa a cikin yanayi huɗu. Kayan aiki na hannu wanda ke ganin gishirin hanya. Shigarwa na bakin teku ko na bakin teku. Kayan abinci da ke zubar da kayan aiki kullum. Da duk wani kaya da ya ratsa teku a cikin kwandon karfe. Idan mai dacewa zai zauna jika na makonni, zinc-nickel shine mafi arha a cikin rayuwarsa.
Dukansu layukan suna farawa iri ɗaya ne. C45 carbon karfe sassa ana inji, dereased a cikin wani alkaline wanka, sa'an nan picked a cikin acid zuwa tsiri oxide. Ƙananan sassa madaidaiciya suna gudana a cikin ganga. Hannun hannu, tees da kayan ɗamara mai girman kai suna rataye a kan tarkace don kowane wurin zama na mazugi ya sami ko da ɗaukar hoto. Daga wannan lokacin, layukan biyu sun bambanta.
Layin zinc yana gudanar da wankan zinc na alkaline, sannan wucewar chromium trivalent. Kaurin ajiya yana ƙasa a kusa da 5 zuwa 8 microns akan daidaitattun sassa. A cikin majalisar feshin gishiri na ASTM B117, tsarin yawanci yana riƙe da tsatsa na kusan awa 96. Jan tsatsa yana biye da kyau kafin sa'o'i 240. Wannan ingantaccen tsari ne, mai ƙarancin farashi wanda ya kare adaftar hydraulic shekaru da yawa. Iyakokinsa suna nunawa kamar farin foda da tsatsa suna fure bayan hunturu ɗaya ko biyu a waje.
Sassan da ke sama da 1000 MPa ƙarfi, galibi ferrules, suma suna tafiya ta hanyar gasa na hydrogen de-embrittlement a kusan digiri 190 zuwa 200 C. Wannan matakin ya shafi duka layin.
Layin zinc-nickel ya haɗa haɗin gwal na kusan kashi 12 zuwa 15 na nickel daga wanka na alkaline. Wannan rabon nickel yana canza komai. Rufin ya fi girma, ya fi iri ɗaya a cikin zaren, kuma yana samar da shinge mai tsayayye wanda ke ƙin lalata daga ciki zuwa waje. Takaddun bayanai a Ruihua Hardware shine 8 zuwa 12 microns na zinc-nickel, wanda aka tabbatar a awanni 240 na ASTM B117 kafin tsatsa ta bayyana.
Har ila yau, gami yana wasa da kyau tare da makwabta. Zinc-nickel yana zaune kusa da aluminum akan sikelin galvanic, don haka yana lalata ƙasa da ƙarfi inda zaren kayan aiki a cikin gidaje na aluminum ko manifolds. Hakanan yana jure yanayin zafin sabis a kusa da digiri 120 C, inda a fili tulin rufin zinc ke raguwa da sauri.
Yi gaskiya game da abin da lambar ke nufi. ASTM B117 tana gudanar da hazo na sodium chloride kashi 5 cikin 100 a digiri 35 na C, a ci gaba, a wani ɓangaren rataye. Kayan aiki ne na kwatanta, ba kalandar rayuwa ba. Daidaitawar da ta wuce sa'o'i 240 a cikin majalisar ba zai rayu tsawon kwanaki 240 a waje ba, saboda abrasion, kimiyyar sinadarai da UV duk suna ƙara hanyoyin kai hari majalisar ba ta taɓa gani ba.
Abin da ƙimar sa'o'i 240 ya gaya muku shine wannan. Lokacin da kwantena na kayan aiki ya zauna a cikin danshi na tsawon makonni shida, sassan zinc-nickel suna fitowa da tsabta yayin da sassan da aka yi da zinc na iya nuna tsatsa mai fari kafin a sanya su. Lokacin da ma'aikatan kulawa ke wanke injin kowane motsi, murfin gami yana kiyaye shingen sa maimakon yin foda. Ƙididdiga yana siyan ku gefe, kuma gefe shine ke raba daidai da kuka maye gurbin a shekara ta shida daga wanda kuka maye gurbin a shekara ta biyu.
Kada ka bari mai siyarwa yayi magana da kai cikin zinc-nickel akan komai. Waɗannan su ne lokuta inda zinc plating shine madaidaicin ƙayyadaddun bayanai:
Kafaffen rukunin wutar lantarki na masana'antu a cikin gida, a cikin masana'anta ba tare da wanke-wanke yau da kullun ba.
Kayayyakin ajiya da kayan haja waɗanda ke zaune a busasshen ma'aji kuma ana amfani dasu cikin watanni.
Gwaji da kayan aikin gwaji da benci waɗanda ba su taɓa barin taron ba.
OEM mai girma yana gina inda ake siyar da injin a cikin bushewar yanayi kuma OEM yana da bayanan filin don mayar da ita.
A kan waɗancan sassan, kashe kuɗin da aka ajiye akan taron da ya dace. Adaftar JIC madaidaiciya 2J da aka yi da zinc da aka sanya tare da zaren tsafta da madaidaicin juzu'i zai wuce abin da ya dace da zinc-nickel wanda aka giciye kuma ya bar sako-sako. Rufi ɗaya ce mai canzawa, ba duka amsar ba.
Yanzu juya tsabar kudin. Ƙayyade zinc-nickel lokacin da aƙalla ɗaya daga cikin waɗannan gaskiya ne:
Na'urar tana aiki a waje duk shekara, musamman ma inda tituna ke da gishiri.
Shigar yana zaune a cikin 'yan kilomita kaɗan daga bakin tekun.
Tushen yana wanke kayan aiki kowace rana ko yana gudanar da zagayowar tsaftacewa.
Sassan suna jigilar ta teku kuma suna iya jira a cikin akwati na makonni kafin shigarwa.
Zaren da ya dace ya shiga cikin aluminum, kuma kuna son jinkirin harin galvanic.
Ga waɗancan ayyukan, ma'aunin ma'aunin ma'aunin bututu a cikin jerin 50011 kyakkyawan ma'ana ne. Suna haɗa bututun ƙarfe zuwa tiyo ta DIN 2353 da ISO 8434-1, wanda aka yi daga karfe C45 tare da 8 zuwa 12 microns na zinc-nickel, ana samun su a cikin jerin haske zuwa mashaya 315 da jerin nauyi zuwa mashaya 630. Kirjin wayar hannu ko injin tashar jiragen ruwa shine ainihin aikin da aka rufa musu.
Ya kamata ku iya tabbatar da murfin bayan sassan sun zo, ba kawai aminta da zance ba. Ruihua Hardware ya yi alamar alamar tambarin akwatin, kuma ana samun takaddun shaida akan buƙata. Idan zane ya kira zinc-nickel zuwa 240 h a kowane ASTM B117, kiran kiran yana canjawa zuwa odar siye da takaddun shaida, don haka binciken ku mai shigowa yana da wani abu don bincika.
Hanya ɗaya mai amfani: sassan layi biyu sunyi kama da akwatin. Dukansu azurfa ne na ƙarfe tare da fa'ida bayyananne. Kar a dogara da gwajin ido. Ajiye alamomin tare da bins, ko canjin kulawa na gaba zai haɗu da haja a cikin wata guda.
Matakin plating da kansa yakan biya sau biyu zuwa sau uku don zinc-nickel, saboda gishirin nickel da tsananin sarrafa wanka suna da tsada. Plating wani ɓangare ne kawai na ƙimar ɓangaren da aka gama, kodayake, don haka akan adaftar C45 da aka ƙera ƙira yawanci yana motsawa ta ƙaramin kaso, ba mai yawa ba. Nemi zaɓuɓɓukan biyu akan RFQ ɗaya kuma kwatanta farashin ɓangaren da aka gama.
Ee. Dukansu nau'ikan hadaya ne akan karfe C45 guda ɗaya, kuma ba sa haifar da matsalolin galvanic da juna. Daidaita sassan zinc-nickel inda danshi da gishiri a zahiri sun isa kayan aiki, kuma platin zinc yana da kyau a wani wuri a kan wannan da'ira.
A'a. ASTM B117 gwajin gwaji ne na kwatanta a cikin hazo gishiri kashi 5 a digiri 35 na C, yana ci gaba da gudana. Rayuwar filin ta dogara da mitar wankewa, gishirin hanya, abrasion da kauri, don haka 240 h a cikin majalisar ba za a iya canza shi zuwa watanni a waje ba. Yana gaya muku yadda shafi ɗaya ke kwatanta da wani ƙarƙashin zagi iri ɗaya.
A gefen ma'auni DIN 2353, jerin irin su 50011 tsayawa tsaye ana kawo su tare da 8 zuwa 12 microns na zinc-nickel, wanda aka kiyasta 240 h a cikin gishiri. JIC adaftan kamar 2J madaidaiciya jirgin ruwa tare da zinc plating a matsayin misali. Ana iya ƙayyade ko wane layi a matakin ƙididdigewa, don haka bayyana yanayin lokacin da kuke buƙatar ƙima.
Faɗa mana inda kayan aikin za su rayu kuma za mu faɗi abin da ya dace, ba mafi tsada ba. Bincika cikakken kewayon akan samfurori page , duba da 50011 madaidaicin bututun tsaye ko kuma 2J madaidaiciya adaftar JIC , sannan aika RFQ ɗin ku ta hanyar shafin tuntuɓar . Ruihua Hardware yana amsawa tare da zaɓuɓɓukan shafi, farashi da lokutan jagora a cikin rana ɗaya ta aiki.
Zinc-Nickel vs Zinc Plating akan kayan aikin Hydraulic: Inda Ainihin Kuɗi ke tafiya
Metric vs BSP na'ura mai aiki da karfin ruwa Threads: 5 Checks Kafin Ka yi oda
6C Metric Bulkhead Fitting - DIN 2353 Girman Girman Panel da Matakan Shigarwa
1EN Metric Male O-Ring / NPT Madaidaicin Adaftar Ruwa - Takaddun bayanai & Jagorar Siyayya
Jagorar Ganewar Ƙaƙwalwar Ma'aunin Ruwa: Zare, 24° Cones da L/S Series
2J Madaidaicin JIC Namiji / JIC Adaftar Ruwa na Mata - Girman Takaddun Bayanai & Jagoran Siyayya
1J9 90° JIC Namiji 74° Mazugi Adaftar Ruwa - Takaddun bayanai, Girman & Jagoran Siyayya
Nau'in Gyaran Jirgin Ruwa da Aka Bayyana: Zaren, Hatimi da Zaɓin
Duban Kayayyakin Kayayyakin Kayayyakin Kayan Aikin Ruwa don Abokin Ciniki na Turai
Metric Standpipe Madaidaicin Fittings - DIN 2353, 50011 Series