Kuna nan: Gida » Labarai da Labarai » Fesa Gishiri Labaran Samfura na Sa'o'i 240 akan Maganar Haɗin Ruwa: Karɓa ko Aika Shi Baya

Gishiri Fesa Sa'o'i 240 akan Maganar Haɗin Ruwa: Karɓa Ko Komawa

Ra'ayoyi: 1     Mawallafi: Lynn Liu Lokacin Bugawa: 2026-11-10 Asalin: Shafin

Tambaya

facebook button sharing
twitter sharing button
maɓallin raba layi
wechat sharing button
linkin sharing button
maballin rabawa pinterest
whatsapp sharing button
share wannan button sharing

Maganar batch ɗinku na sake fasalin ya ce gwajin feshin gishiri: awanni 240, ASTM B117. Kayan aiki suna zaune akan tashar jirgin ruwa, injin yana ƙasa, kuma alamar akwatin tana maimaita lamba. Yawancin masu kula da kulawa suna sa hannu a kan sa, saboda lambar tana kama da bayanai. Wannan labarin yana ɗaukar layi mai ƙarfi: sa'o'i 240 layin wucewa ne, ba alƙawari ba, kuma bincike guda biyar sun yanke shawarar ko rukunin ya sami hanyar shiga cikin shagunan ku.

Aika shi baya ko sanya shi a kan shiryayye - layin yana iya jawowa. Gudanar da jeri cikin tsari: duba ɗaya akan kalmomin da'awar, ɗaya akan ma'aunin wucewa, ɗaya akan kauri, ɗaya akan takarda, ɗaya akan sassan kansu. Babu ɗayan biyar ɗin da ke buƙatar dakin gwaje-gwaje. Ruihua Hardware yana jigilar waɗannan cak guda biyar, wanda shine dalilin da ya sa suke karantawa kamar tsarin dubawa da aka rubuta daga wancan gefen benci.

WechatIMG30775.jpg

Matsayin: Sa'o'i 240 Layin Wuta ne, Ba Alƙawari ba

Na farko, san abin da majalisar ke yi. ASTM B117 tana fesa hazo na 5 na sodium chloride a 35 ° C, ci gaba, a wani ɓangaren rataye. TS EN ISO 9227 NSS yana bayanin feshin gishiri iri ɗaya a cikin kalmomi daban-daban. Gwajin kayan aiki ne na kwatanta. Yana gaya muku yadda shafi ɗaya ke yi da wani a ƙarƙashin irin wannan cin zarafi marar iyaka. Ba ya gaya muku kwanan wata.

Don haka ku dage da wuri. Duk wata magana da ta canza sa'o'i 240 zuwa 'shekarun rayuwar filin' tana siyar da ku lambar da gwajin ba zai iya samarwa ba. Chemistry na wanke-wanke, gishirin hanya, abrasion da UV duk buɗe hanyoyin kai hari majalisar ba ta taɓa gani ba. Karɓar sa'o'i 240 azaman kofa da kuke riƙe masu siyarwa, batch da batch da lulluɓi da sutura. Karɓar kowace fassarar sa'a ta ƙidaya zuwa kalanda. Wannan matsaya ita kaɗai ce ke kashe mafi yawan muhawara kafin su fara.

Mataki na 1: Neman Ma'auni, Ba Magana ba

Karanta da'awar akan kalma kalma da kalma. Kiran da ake iya tabbatarwa yana ɗaukar abubuwa huɗu: daidaitaccen suna (ASTM B117 ko ISO 9227 NSS), ƙidayar sa'a, ma'aunin wucewa, da shafi tare da kauri. 'Zinc-nickel 8-12 μm, babu ja bayan sa'o'i 240 a kowace ASTM B117' shine da'awar. 'An gwada feshin gishiri' taken magana ne, kuma ba za a iya bincika ko maimaita ko jayayya da taken ba lokacin da haɗin gwiwa ya yi kuka a cikin wata goma sha ɗaya.

Saita ƙa'ida da ƙarfi: ƙididdiga da ba ta suna ba ƙaramin farashi ba ne, da'awar da ba za a iya tabbatarwa ba ce. Aika RFQ baya kafin aika odar siyayya. Wasiƙar amsa ɗaya ta gyara shi; sake fasalin kasa ba ya yi.

Mataki na 2: Karanta Ma'anar Wuta - Farin Tsatsa Ba Ja Bane

Ƙididdigar sa'a ba ta nufin kome ba har sai kun san abin da ake ƙidaya a matsayin gazawa. Farin tsatsa shine furen lalatawar zinc a saman. Yana kama da mara kyau kuma baya yin cutarwa; shine matakin farko da ake tsammanin akan kowane tsarin zinc. Jan tsatsa ne tushe karfe lalata, kuma shi ne inda shafi ya kasa a zahiri.

Don haka ma'aunin da ka karɓa dole ne ya kasance bisa ja-tsatsa lokacin da dacewar ke aiki a waje. Don ƙayyadaddun zinc-nickel, layin shine 'babu ja a cikin sa'o'i 240'. Fuskar haske mai haske a cikin awa 240 akan wani yanki mai wucewa ba gazawa ta atomatik ba. Don ma'auni na zinc plating, lissafin lissafi ya bambanta da gaskiya: tsarin zinc a cikin kewayon 5-8 μm yawanci yana riƙe da tsatsa mai tsatsa na kimanin sa'o'i 96, kuma tsatsa ja ya zo da kyau kafin 240. Wannan al'ada ne ga tsarin, ba dalili ba don ƙin yarda - shi ne filaye don kiyaye sashi a cikin gida. Yanayin gazawar da kuke jurewa yana yanke hukunci, don haka rubuta ma'aunin kafin jigilar kaya, ba bayan ba.

Mataki na 3: Daura Sa'o'i zuwa Kaurin Rufe

Awanni ba tare da kauri ba rabin ƙayyadaddun bayanai ne. Abubuwan ajiya na 8-12 μm zinc-nickel suna ɗaukar sa'o'i 240 a cikin majalisar; adibas na 5-8 μm zinc yana ɗaukar kusan 96. Rahoton da ya yi iƙirarin sa'o'i 240 akan ajiya na 3 μm yana kwatanta wani tsari, ko kuma wani mai kaya.

Tabbatar da gefen ku. Ma'aunin shigar da maganadisu yana karanta sashin ƙarfe na carbon da aka sadaukar da kyau sosai don yanke shawarar tashar jirgin ruwa, kuma mita XRF tana karantawa ba tare da yanke ba. Ɗauki karatu uku a kowane bangare: wurin zama na mazugi, cikin zaren gudu, da shank. Kwatanta ƙaramin karatun da taga kauri akan takaddun shaida. Ƙarƙashin ƙaƙƙarfan abin da aka bayyana, ƙi amincewa da rukunin ba tare da la'akari da abin da rahoton ya ce ba - rahoton ya kasance mai gaskiya ne kawai kamar hanyar haɗin gwiwa zuwa sassan da ke gaban ku.

Mataki 4: Bi Takardu Daga Zane zuwa Label ɗin Akwati

Takaddun lalata kawai yana kare ku idan ya tsira daga dukkan sarkar: kiran kiran zane yana canjawa zuwa odar siye, odar siyayya zuwa tsarin samarwa, tsari zuwa lakabin akwatin, da akwatin zuwa takardar shaidar tsari. Katse hanyar haɗin gwiwa guda ɗaya kuma binciken da ke shigowa ba shi da wani abin dubawa a kai.

Ruihua Hardware yana yin alamar alamar tambarin akwatin kuma yana ba da takaddun shaida akan buƙata, don haka kira kamar 'Zn-Ni 8–12 μm, 240 h a kowane ASTM B117' ya zo a rubuce akan kowane Layer na jigilar kaya. Riƙe masu samar da ku zuwa sarkar iri ɗaya. A kan aikin sake fasalin ko OEM wanda ke buƙatar ganowa, tsari ba tare da takaddun shaida ba shine riƙewa, ba ƙin yarda ba kuma ba karɓa ba - sassan suna jira har sai takarda ta kama. Ajiye takalmi tare da bins kuma; tsarin sutura guda biyu sunyi kama da akwatin, kuma motsi na gaba zai haɗu da su a cikin wata guda.

Mataki na 5: Binciken Dock - Abin da Kuna Iya Yin Hukunci Ba tare da Lab ba

Duban ƙarshe yana ɗaukar mintuna goma kuma ya sami mafi yawan abin da ke da mahimmanci. Yi aiki ta hanyar buɗaɗɗen katun ta wannan tsari:

  1. Kariyar zaren.  Kowane ƙarshen zaren yana ɗaukar hula ko filogi. Zaren da ba a taɓa gani ba a cikin ɗanɗano mai ɗanɗano yana ɗaukar furen farko kafin a taɓa shigar da sashin.

  2. Launi da daidaituwa.  Dukansu tsarin sutura suna fitowa da azurfa iri ɗaya. Launi mai launin toka, faci mai gizagizai ko adibas kamar foda a cikin zaren sun cancanci kallo na biyu.

  3. Babu ja a ko'ina.  Bincika kujerun mazugi, bores da tushen zaren don tabo ja. Ɗayan ɓangaren ja shine ƙararrawar samfurin ga duka rukuni.

  4. Rufe kan sassa masu rikitarwa.  Hannun hannu da tees suna rataye a kan tarkace yayin plating don haka kowane mazugi yana samun ko da ajiya. Fuskar mazugi a gwiwar hannu ta ce ɗaukar hoto ya kasance siririn inda ya fi dacewa.

  5. Takaddun suna cikakke.  Tambarin akwatin da za a iya karantawa, plating spec leable, lambar tsari yanzu. Babu lakabi, babu ganowa, babu takaddun shaida daga baya.

Idan ƙayyadaddun ya ƙunshi sassa masu ƙarfi irin su ferrules sama da 1000 MPa tensile, kuma tabbatar da gasa ta hydrogen de-embrittlement an bayyana - 190 zuwa 200 ° C bayan plating, akan duka zinc da zinc-nickel line.

Karɓa, Lura, ko Ƙi: Ƙaddamarwa

Nemo a tashar jirgin ruwa ko a kan fa'ida

Hukunci

Matsayin sunaye daidai + sa'o'i + ma'aunin ja-tsatsa + kauri; sassan sun wuce duban jirgin ruwa

Karba

Farin farin haske mai haske akan sassan da aka yi da zinc, ƙayyadaddun ƙayyadaddun tutiya ne

Karɓa tare da bayanin kula  - al'ada don tsarin; ajiye sassan a cikin gida

Ma'auni ya ɓace daga cikakkiyar da'awar in ba haka ba

Riƙe  - sami ma'auni a rubuce kafin sassan su hau kan na'urar bakin teku ko ta hannu

Babu takardar shedar tsari akan aikin ganowa

Riƙe  - sassan jira har sai takarda ta kama

Ƙaunar kauri ƙasa da mafi ƙarancin da aka bayyana

Karɓa  - rahoton bai bayyana wannan rukunin ba

Jan tsatsa a kowane bangare a ƙarƙashin kira na zinc-nickel na awa 240

Karɓa  - rukunin ya gaza layin wucewa na kansa

Quote ya ce kawai 'An gwada feshin gishiri'

Aika RFQ baya  - da'awar ba ta da tabbas kamar yadda aka rubuta

Abin da Ruihua Hardware Ke Sanya A Bayan Lamba na Sa'o'i 240

Bututun tsaye na 50011 kai tsaye a cikin kewayon Hardware na Ruihua shine sashin tunani na wannan gabaɗayan hanya. Yana haɗa bututun ƙarfe zuwa tiyo ta DIN 2353 da ISO 8434-1, wanda aka ƙera daga C45 carbon karfe tare da 8-12 μm na zinc-nickel, ba tare da jan tsatsa ba a sa'o'i 240 na ASTM B117, a cikin jerin haske zuwa mashaya 315 da jerin nauyi zuwa mashaya 630. Kirjin tashar jiragen ruwa, mai lodin tirela mai gishiri a hanya ko layin abinci mai wanke-wanke yau da kullun shine ainihin aikin da aka lullube shi. Duba cikakken jerin girman akan 50011 jerin shafi.

Bangaren bambanci na ganganci ne. The 2J madaidaiciya JIC adaftar  jiragen ruwa tare da trivalent zinc plating a cikin kewayon 5-8 μm, rike da farin tsatsa zuwa kusan sa'o'i 96 - daidai, daidai-farashin amsa ga tsayayyen wutar lantarki a cikin gida. Inda kowane layin shafi ke samun ƙimar sa shine tambayar kuɗi, kuma labarin da ya gabata akan zinc-nickel da zinc plating  yana tafiya ta ciki. Wannan labarin ya shafi sauran rabin: da zarar an ƙayyade abin rufewa, ga yadda mai siye ke tabbatar da shi.

Menene Masu Kula da Kulawa suke Tambaya Game da Da'awar Fasa Gishiri?

Shin sa'o'i 240 na feshin gishiri yana nufin adadin adadin shekaru a waje?

A'a. Majalisar ministoci tana gudanar da hazo na gishiri kashi 5 a 35 ° C ci gaba; filin ba. Bi da sa'o'i 240 a matsayin kofa na kwatanta tsakanin sutura da batches, kuma ƙi kowane juyi zuwa shekarun filin.

Shin farar tsatsa akan kayan gyara masu shigowa an ƙi?

Ba da kanta ba. Farin furanni shine mataki na farko da ake tsammanin akan tsarin zinc, don haka haske mai haske akan daidaitaccen ɓangaren zinc shine karɓa-tare da bayanin kula. Jan tsatsa shine layin ƙi. Ƙarƙashin kiran sa'o'i 240 na zinc-nickel, fure mai nauyi tare da jajayen tabo shine riko-da-nema-takardar shaida.

Wane ma'auni na izinin siyan ya kamata ya ɗauka don aikin bakin teku?

Zinc-nickel 8-12 μm, babu jan tsatsa bayan sa'o'i 240 ta ASTM B117 ko ISO 9227 NSS. Layi ɗaya, ana iya canjawa wuri daga zane zuwa PO zuwa lakabin akwatin zuwa takardar shaida.

Zan iya duba kauri ba tare da dakin gwaje-gwaje ba?

Ee. Ma'aunin maganadisu akan ɓangaren sadaukarwa ko mita XRF akan ɓangaren da aka ajiye. Karanta wurin zama na mazugi, zaren gudu da shank, kuma kwatanta mafi ƙanƙanta da taga takardar shaida.

Maganar kawai ta ce 'An gwada feshin gishiri' - karba?

Tukuna. Nemi daidaitattun, awoyi, ma'auni da kauri a rubuce. Mai sayarwa tare da ainihin shirin fesa gishiri yana ba da amsa a cikin ranar aiki; daya ba tare da shi ya riga ya amsa tambayar ku ba.

Aika Da'awar, Ba kawai Lambar Sashe ba

RFQ na gaba, sanya kiran kira a cikin bayanin kula kafin fara tattaunawar farashin: shafi, kauri, daidaitaccen, sa'o'i, ma'auni. Aika shi zuwa Ruihua Hardware ta hanyar shafi na lamba  tare da yanayin aiki da aka bayyana a cikin layi ɗaya, kuma ƙididdiga ta dawo tare da ƙayyadaddun bayanan plating akan lakabin akwatin da zaɓin takardar shaidar riga an farashi. Cikakken kewayon dacewa yana zaune akan samfurin page . Rukunin da zaku iya tantancewa akan tashar jirgin ruwa shine kawai nau'in da ya cancanci sanya hannu akai.

Zafafan Kalmomi: Kayan Aikin Ruwa,  Kayan Aikin Ruwa na Ruwa, Hose da Fittings,   Na'ura mai aiki da karfin ruwa Quick Couplings , China, masana'anta, mai kaya, masana'anta, kamfani
Aika tambaya

Kashi na samfur

Tuntube Mu

 Tel: +86-574-62268512
 Fax: +86-574-62278081
 Waya: +86- 13736048924
 Imel: ruihua@rhhardware.com
 Ƙara: 42 Xunqiao, Lucheng, Yankin Masana'antu, Yuyao, Zhejiang, China

Sauƙaƙe Kasuwanci

Ingancin samfur shine rayuwar RUIHUA. Muna ba da samfurori ba kawai ba, har ma da sabis ɗinmu na bayan-tallace-tallace.